316 Stainless Steel Pipe & Tube: Molybdenum-Enhanced Chloride Corrosion Resistant Piping

Jan 30, 2026

Ostavi poruku

What is 316 Stainless Steel Pipe & Tube?

316 stainless steel pipe is a molybdenum-containing austenitic piping product, upgraded from 304, with significantly improved chloride corrosion resistance, suitable for coastal, marine and weak corrosive industrial scenarios.

UNS: S31600|JIS: SUS316|GB: 06Cr17Ni12Mo2|EN: X5CrNiMo17-12-2|W.Nr.: 1.4401

C: <=0.08|Si: <=1.00|Mn: <=2.00|P: <=0.045|S: <=0.030|Cr: 16.00-18.00|Ni: 10.00-14.00|Mo: 2.00-3.00|Fe: Balance

Key Properties (20℃, Annealed, Horizontal)

Density: 7.98g/cm³|Melting Point: 1375-1450℃|Tensile Strength: 515-690N/mm²|Yield Strength: >=205N/mm²|Elongation: >=40%|Hardness: <=217HB

• Molybdenum-boosted corrosion resistance: Effectively resists pitting and crevice corrosion from chloride ions • Excellent processability: Easy to form and weld, suitable for complex pipeline structures in corrosive environments • Stable medium-temperature mechanics: Balances toughness and strength for industrial process piping • Wide corrosive scenario adaptability: Applied in marine engineering, chemical processing and coastal architecture

  C P S N
316 - - - 0 - 16.0 2.00 10.0 -
0.08 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316L - - - - - 16.0 2.00 10.0 -
0.03 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316H 0.04 0.04 0 - - 16.0 2.00 10.0 -
0.10 0.10 0.75 0.045 0.03 18.0 3.00 14.0 -

 

If you have project requirements for stainless steel, we welcome your order. GNEE has a large inventory of popular products for you to choose from. It can be processed into various practical product forms, including plates, coils, tubes, bars, wires, etc. For detailed chemical composition information and free samples, please contact our factory immediately. We offer competitive prices and excellent service.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Testing and Documentation: Factory test certificate, EN 10204 3.1, chemical report, mechanical report, destructive testing report, non-destructive testing report, PMI test report, visual inspection report, third-party inspection report, NABL certified laboratory report.
Packaging: Wooden crate packaging, bubble wrap packaging, steel strapping, or packaging according to customer requirements.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Pošaljite upit